Resists sea water, steam, salt and caustic solutions. Used in heat exchangers. Other Monel available.
Basic Composition: Ni 67%, Cu 28%, F3 3%, Mn 2%
Temperature Limits: 0 to 480 ° C
International Standards: UNS N00440
Density: 8.84g/cm³
Melting Range: 1320 ° C
Specific Heat: 430 J/Kg ° C
Coefficient of Expansion: 14 x10-6 / ° C